The Nylon 6,6 provided the highest average rubber retention in primary adhesion and environmental testing, which is consistent with the frequent use in the industry today.
Primary adhesion was evaluated using ASTM D 429 Method F buffer specimens.
Figure 1 shows the effect of dilution of 8110 on primary adhesion for six different rubbers cured for seven minutes at 191 degrees C.
The bonded parts were tested for primary adhesion and exposed to 5% salt spray for three and seven days.